| dc.description.abstract |
Steel production through electric arc furnace (EAF) technology has emerged as an essential
process in contemporary metallurgy, particularly in terms of its adaptability and resource
flexibility. The EAF represents one of the most prevalent methods for steel manufacturing,
primarily utilized in the casting and rolling phases within steel plants. The inception of the first
EAF dates back to the early 20th century. The inherent versatility of the electric arc furnace allows
it to cater to the dynamic demands for steel materials, which has facilitated the development of
mini steel plants focused on producing various grades of steel products from steel scrap and
alternative charge materials.
In EAF operations, steel scrap serves as the principal raw material; however, challenges such as
limited scrap availability and the need for low-residual or high-purity iron sources have
necessitated the incorporation of direct reduced iron (DRI), hot briquetted iron (HBI), pig iron,
and hot metal in the steelmaking process. Significant advancements in the operational aspects of
EAF steel production have enhanced its contribution to global steel output. According to the
World Steel Association, electric arc furnaces account for approximately 30% to 35% of the total
steel production worldwide. Over the past three decades, numerous innovations in EAF
steelmaking have been implemented to minimize power consumption, optimize tap-to-tap timings,
reduce electrode usage, and lessen refractory wear.
This study critically analyzes the steelmaking and refining processes employed at AbulKhair Steel
(AKS) melting plant in Bangladesh. An examination of the significance of raw materials in the
steelmaking process forms a central component of this research. Various parameters, including
specific electrical energy consumption, tap-to-tap timing, lime consumption, carbon consumption,
and electrode consumption, were examined across four distinct charging mixture ratios (MR). A
comparative analysis of these parameters was conducted graphically, with a focus on determining
the most cost-effective and productive mixture ratio for the steelmaking process. Among the
evaluated mixtures, the MR-2, consisting of 87.7% scrap (comprising 67.7% shredded scrap and
20% heavy melting scrap) and 12.3% pig iron, demonstrated the most favorable results,
establishing its efficiency relative to the other raw material mixtures examined. The findings
indicate that the lowest specific power consumption, tap-to-tap (TTT), and electrode consumption
were recorded for MR-2, in contrast to the other ratios. In contrast, MR-4 exhibited the highest
specific electrical energy consumption, TTT, lime consumption, and electrode consumption.
Interestingly, carbon consumption was highest in MR-1, which contained a significant amount of
scrap with 10% hot briquetted iron (HBI) and 5% pig iron. The presence of FeO in HBI
necessitates greater carbon consumption to produce carbon monoxide (CO) gas. |